LEARNING CURVE 8

The endliner, made of Queensland Kauri,  is now installed along the inside edge of the lute body – where the construction is at its weakest.

Later on I will glue an endclasp to the outside edge, for additional strength.

I am pleased to report that the little wooden clamps did their job perfectly well. It seems they are not merely charming to look at, but more or less functional….